Al2O% - 23% Opira ma ok ti gi seramik

Al2O% - 23% Opira ma ok ti gi seramik

1. Gima nitie e alumina en 17% - 23%, kit ball ma ok nyal tiyo;
2. Nengo mapiny, tiyo gi yore mang'eny, weche ma mulo piny mangima, kod rito mayot;
3. Otiyogo ahinya kaka gik ma konyo e gik ma kelo katalitik kod gik ma ng’ato nyalo ng’ado e bwo gik ma ng’ato nyalo timo e yor kemikol.
Chiwo penjo
Kit gimoro
Pamek mag teknoloji

10:10, 11. 10 En achiel kuom jogo ma nyalo loso kendo chiwo ball ma ok nyal tiyo gi al2o 3 17%-23% e piny China. Ka wan gi ng’eyo mang’eny, warwako gi mor mondo inyiew ball ma nigi ng’injo ma malo mar al2o 3 17%-23% ma ok nyal ng’injo ma inyalo uso kae kuom kambi marwa. Tudri kodwa mondo iyud sampol ma nono.

 

Yangruok

 

17-23% alumina ma ok nyal tiyo gi ball mar seramik, nyiso gik ma seramik ma ng’injo ma olosi ahinya gi sistem mar siliket ma nigi alumina matin ahinya (ma pile 17-23% Al2O3), ma iloso kokalo kuom ng’injo ma nigi liet ma malo -. En kit ball ma ok nyal tiyo gi alumina ma itiyogo ahinya.

 

17% -23% alumina ma ok nyal tiyo gi ball mag seramik miyo ng’ato geno kendo keto gik ma nyalo ketho piny e bwo ng’ich ma ng’ich, ng’ich ma ng’ich, kod gik ma ok ng’ich ma nyalo ketho ng’ich. Ok gin gi gombo mar bedo gi ng’ich ma malo ahinya kata bedo gi teko ma malo ahinya, to ginyalo chopo dwaro mag konyo kod keto gikmoko e bwo gik ma pile pile mag injinia mar kemikol.

 

Kaka gik ma itiyogo e loso gik moko, ball mar alumina ma ok nyal tiyo gi pesa mang’eny ong’ere ahinya nikech nengo mare ma piny kendo tiyo gi yore mang’eny. 17-23% mar ball mag seramik itiyogo ahinya e gik ma kelo ng’injo kod gik ma ng’injo mondo ogeng’ ng’injo mar ng’injo mag molekul kod silika gel. Bende, inyalo tiyo kodgi kaka gik ma ok nyal tiyo e tower mag keto kemikol kod gik ma itiyogo mondo ilos kaka gas kata pi ng’ado.

17 23 inert ceramic ball
al2o3 17 23 ceramic ball
17 23 alumina ceramic ball

 

Weche mag Teknikal

 

Kido

17% - 23% mar alumina ma ok nyal tiyo

Neno

Opira marachar

Al2O3+SiO2(%)

>93

Al2O3(%)

17-23

Fe2O3(%)

<1

CaO (%)

<0.5

MgO (%)

<0.5

TiO2(%)

<0.5

K2O+Na2O(%)

<4

H2O Ywayo (pek.%)

<0.5

King' mar mwandu mang'eny (g/ml)

1.3-1.4

Teko mar Mohs (rapim)

>6.5

Teko mar liet (digri)

>1300

Nyalo mar kwedo asid (%)

>98

Nyalo mar alkali (%)

>80

Teko mar Ketho (KN)

Inji 1/4 (milimita 6)

>0.5

Inji 1/2 (milimita 13)

>1.5

Inchi 3/4 (milimita 19)

>4.15

Inchi 1 (milimita 25)

>6.07

Inchi 1-1/2 (milimita 38)

>8.52

Inchi 2 (milimita 50)

>9.7

 

 

Tich mare

 

  • Suport mar Mekanik mar Ohala Ne Katalis Kata Gik Mamulo Pi

 

 

Nods mag Hoot: 23% ball mar seramik ma ok nyal tiyo, 17% 23% mar seramik ma ok nyal tiyo, Al2O3 17% 23% mar seramik, 17% 23% mar seramik ma ok nyal tiyo, 17% 23% mar seramik mar alumina, China

Chiwo penjo
Chiwo penjo